ASI Magazine
  Home
  ASI Green
  Subscribe
  eNewsletter Subscription
  Subscription Customer Service
  Updates
  Calendar of Events
  Call for Papers
  Features
  Columns
  Today's Headlines
  Price Adjustments
  New Products
  Ad Index
  Podcasts
  Ask Dr. Dave
  ASI Blog
  Online Exclusives
  Adhesives in the News
  Resources
  Books
  Archives
  Digital Edition Archives
  Classified Ads
  Career Center
  Tech ManufactureXPO
  Industry Links
  Online Solutions Web Seminars
  This to That
  Services Marketplace
  E-Newsletter Archives
  Green Opportunities E-News Archives
  Market Research
  Literature Showcases
  Glossaries
  Directories
  ASI Info
  Media Kit
  Contact Us
  Sales Staff
  Reprints
  List Rental
Search in: EditorialProductsCompanies
Protecting Building Aesthetics
by Larry Carbary
April 1, 2008

ARTICLE TOOLS
EmailEmailPrintPrintReprintsReprintsshareShare



Dow Corning sealants are featured in the weatherproofing of the glass curtainwalls of the Time Warner Center in New York City. RSG Caulking & Waterproofing, one of the largest caulking installation companies in New York, has successfully used Dow Corning sealants on almost every project for the past 22 years.
Because the physical condition of a building can change greatly over time due to external forces such as sun, wind and rain, choosing materials that will maximize the life and appearance of the structure, while minimizing the amount of damage, is crucial. This is especially true in selecting a sealant. Following are some of the most common aesthetic issues to consider.
  • Dirt Pick-Up – Accumulation of dirt on a sealant’s surface is particularly prevalent on construction sites with large amounts of dust. The actual amount of dirt pick-up will vary with exposure conditions, but excessive pollutant contamination will result in lower durability and weaker bond strength. To avoid this, choose a sealant that can tolerate higher levels of contamination.
  • Chalking – As the substrate begins to degrade and erode over time, the surface becomes more rough and porous, which leads to a loss of surface gloss and color. Chalking is most observed in organic sealants that are initially black or brown, but later transform into a light gray or beige. This does not occur with silicone or acrylic sealants.
  • Change of Color – Color change can result from factors both inherent and external to the sealant. Incompatibility of the sealant with other building materials is a contributing factor. Materials with high incompatibility levels include low-molecular-weight polymers, antioxidants or tar. A sealant that is compatible with a variety of other substrates is preferable.
  • Surface Crazing – A variety of factors, including sunlight, environmental stress and aging, can cause cracks in the sealant’s surface. This is especially common with organic sealants. Generally, sealants with higher polymer content are more durable and less subject to crazing.
  • Fluid Migration – Fluids can migrate from a sealant to the substrate, creating a dark “wet” band look around the joint of the sealant. The extent and rate of fluid migration varies with the type of sealant. Cheaper, less formulated sealants are the most prone to staining and fluid migration.
  • Other Environmental Factors – Oxygen, ultraviolet radiation, climate/temperature, microbial growth and other environmentally-induced mechanisms can contribute to the fatigue and stress that degrades and lowers the overall bond strength of the sealant.
While aesthetic issues cannot be completely avoided, they can be mitigated through prior knowledge; selection of high-quality, high- performance building materials; and working with a reputable manufacturer.


About Dow Corning Construction

For more than 60 years, Dow Corning has provided silicon-based, performance-enhancing materials and additives for glazing, sealing, and weatherproofing new and existing construction projects. For more information, visit www.dowcorning.com/construction.


Larry Carbary
Larry Carbary is a Dow Corning Construction Associate Industry Scientist.