Epoxies, Etc… has developed a new thermally conductive, flame-retardant epoxy potting and encapsulating compound. 50-3150 FR Black Epoxy with Catalyst 190 and Catalyst 105 is listed with Underwriters Laboratory for passing UL 94 V-0. 50-3150 FR is designed to provide electrical insulation while transferring heat away from hot components. In addition to protecting electronic assemblies, it also is a flame retardant and self-extinguishing epoxy system. Other features include low viscosity and excellent heat transfer. 50-3150 FR is available in quarts, gallons, and five-gallon pails.