TRA-BOND 2143D is a medium-viscosity polyamide epoxy adhesive recommended for application where impact resistance and superior mechanical properties are essential. This compound can be room temperature- or heat-cured and features an ultimate Tg of 65 degrees C. 2143D exhibits low moisture absorbance and a high-lap shear strength of 2,200 psi. It bonds well with most metals, rigid plastics, glass, ceramics, leather, rubber and wood.

For more information, visit http://www.tra-con.com or call (800) TRA-CON1.