Improving Polymer Chemistries

With careful research, polymer chemistries can be tailored to end-use applications.



Polymers have been used in the formulation of adhesives for decades. In recent years, the technology base has been optimized and expanded to include a broader range of polymer chemistries. Polymers used for adhesive formulation include water-based acrylic emulsions and solid acrylics, urethane and urethane-acrylic dispersions, and solvent-based polyesters. This later technology is ideal for the lamination of filmic substrates used in flexible packaging. Today, polymers play a major role in the formulation of adhesives for a broad range of applications in other packaging markets such as lidding, labeling, and blister-pack, as well as industrial markets like automotive, general lamination, wood bonding, and consumer markets.

Bottle Labeling

Synthetic polymers are commonly used for paper and polyester labeling substrates. Water-based acrylic copolymers using acid-stabilized colloidal or emulsion technology offer an excellent balance of adhesion and end-performance properties for bottle labeling applications. The main challenge is to balance stable application viscosity (for high-speed filling lines), high-performance adhesive properties and ease of label removal for recycling.

NeoCryl BT-207, a water-based acrylic emulsion, is a viable alternative to natural casein products that have been predominantly used in this market. Historically, adhesive formulators have faced major difficulties when replacing natural casein-based adhesives for bottle labeling applications. Manufacturers of synthetic polymers struggled to match the full performance range and benefits of casein. However, due to issues with supply constraints, consistent quality and the price volatility of casein, there is a real need to find a synthetic alternative.

The performance of NeoCryl BT-207 closes this gap, offering enhanced performance for high-speed stable viscosity over a pH range of 8-8.6 with improved hyper-condensation resistance for cold-fill bottle labeling. In addition, the emulsion is not susceptible to biological attack. The combination of these benefits provides an advantage in the form of overall cost reduction.

Flexible Packaging

The significant growth of filmic substrates for flexible packaging is well known; lightweight alternatives to metal cans offer consumers ease of use and allow for more decorative and attractive graphics that are ideal for point-of-sale and marketing promotions. The package itself is constructed of bonded layers of different filmic substrates, including metalized layers and alumina foils, and incorporates closing mechanisms for ease of storage. The ideal adhesive must achieve universal high bond strength with the different material layers, as well as high performance in a variety of packaging procedures, including pasteurizing and retortable processes.

Using its capabilities and knowledge of polyester chemistry for can and coil coatings, DSM has developed a polyester polymer for use as a high-performance lamination adhesive. NeoRez P-900, a high-molecular-weight, OH-functional polyester polymer, is recommended for use as a universal laminating adhesive for flexible packaging and filmic substrate applications.

This polymer displays excellent adhesion to a broad range of substrates, including co-extruded polypropylene, biaxial-orientated polypropylene and polyester, polyethylene, polyamide, and aluminum. NeoRez P-900 can be formulated to take advantage of the high molecular weight to improve productivity with faster lamination throughput, lower post-curing temperature and a more rapid post-curing time.

Performance can be enhanced with the addition of an isocyanate crosslinker, which can lead to an overall cost reduction due to the lessened amount of crosslinker required to equal the performance of competitive urethane systems. NeoRez P-900 also features high performance and maintains excellent bond strengths under retorting conditions, which makes it ideal as a flexible packaging lamination adhesive and an alternative to commercial crosslinked, solvent-based urethanes. NeoRez P-900 is free of aromatic isocyanate and amine additives in its composition and is compliant with the U.S. Food and Drug Administration’s food contact requirements.

Table 1. Bonding Strength vs. Time and Condition

Heat-Activated Adhesives

Urethane dispersions are used for heat-activated adhesives in industrial lamination processes for the construction of automotive interiors such as dashboards, door trims and roof linings. These dispersions are also used in the manufacture of kitchen cabinets, laminating PVC foils onto MDF board, and rigid plastic lamination of credit card and graphic display panels. DSM Coating Resins uses both pre-polymer and inversion polymerization production techniques to produce a range of urethane dispersions. Careful selection of raw materials and processing conditions yields polymers that are solvent-free, easy to formulate, and feature low activation temperatures and high bond strength (which can be formulated to attain high temperature resistance).

NeoRez R-1400 is an aliphatic polyester urethane polymer dispersion developed for heat-activated adhesive formulation. NeoRez R-1400 offers the combined properties of low temperature activation, good early green strength, and high temperature resistance when crosslinked with poly-dispersible isocyanate.

The polymer imparts high bond strengths and displays excellent adhesion to a variety of materials, including wood, common grades of plastic films, and vinyl laminates. The low activation temperature characteristic of the polymer makes this resin ideal for use in waterborne adhesives that require reduced bonding temperatures (i.e., in applications where temperature-sensitive substrates are used, such as decorative vinyl lamination in automotive interiors and kitchen cabinet assemblies).

Figure 1. Multiple Benefits Provide Overall Cost Reduction

Wood Adhesives

Urea-formaldehyde resins have been used for many years as the workhorse adhesives in wood bonding applications. Inexpensive thermoset urea-formaldehyde is ideally suited to the high performance and long life requirements in applications such as the low-cost, high-volume furniture market and general wood lamination. In today’s market, however, additional focus has been placed on reducing environment impact and maintaining worker safety. The use of formaldehyde is therefore under pressure, and the market is looking for viable alternatives.

NeoPac E-850 is a formaldehyde-free, water-based aliphatic polyester urethane-acrylic dispersion. This system was developed specifically for use in wood furniture adhesives due to its bond strength and excellent water and heat resistance. As a water-based polymer, it can be highly loaded with mineral fillers to reduce the overall water content in the formulated adhesive without loss of adhesion properties. This is a necessary requirement for most wood laminating production methods in controlling viscosity, wood penetration and faster drying.

The product can be used in adhesives to form flat or shaped laminated parts. The nature of the resin imparts the necessary performance to withstand bond stresses in the laminate along bends in the formed components. In addition, it exhibits good water and fatigue resistance properties. The product meets the standards of major flat-pack supplier regulations regarding formaldehyde-free and wood furniture construction performance.

For more information, visit www.dsm.com.

Links

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

Michelle Moss is an industry manager at DSM Coating Resins.
You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI June 2013 cover

2013 June

The 2013 June Adhesives and Sealants Industry Magazine includes articles about Nordson EFD and UV curing with lasers, as well as a case study on progressive cavity pumps. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40