asi0412-DrDave-img-inbody.jpgQUESTION: We want to bond aluminum to several thermoplastics and thermosets for an outdoor application that could experience both high and low temperatures. What types of adhesives should we consider?

ANSWER: A cyanoacrylate adhesive will probably give you rapid high-strength bonds, but you should be careful about the high temperature requirement. Cyanoacrylates are thermoplastic, non-crosslinked adhesives and may creep under load. It is important to test the adhesives under the appropriate conditions.
Epoxies will give you better high-temperature properties—particularly if you heat-cure them—and should perform well on most thermoset plastics. However, you should expect lower strengths than cyanoacrylates on many thermoplastics.

You might also consider trying a reactive acrylic adhesive for this application. This type of adhesive bonds these materials very well and has some toughness and flexibility to resist the stresses caused by differences in the thermal expansion coefficients of the materials you are bonding.
 

QUESTION: Why do some manufacturers of polyurethane sealants say that I should not tool a joint with soap and water (even though to use nothing is almost impossible)? However, they do suggest that open cell backer rods are better than closed cell ones because they allow the moist air to reach the product to help it cure. Why then can’t I use water to finish the joint? I am also seeing mineral spirits mentioned as a finishing product—can I use this?

ANSWER: Most manufacturers do not recommend soapy water for tooling the joint for three reasons. First of all, the soap can sometimes interfere with adhesion. Secondly, excessive moisture in a polyurethane can often lead to CO2 generation and create bubbles in the sealant. You probably noticed that application of these sealants is not recommended if rain is expected. Finally, water can sometimes cause staining of the joint. Dry tooling is usually recommended, but hydrocarbon solvents, such as mineral spirits or xylene, can be used if necessary.

 


Any views or opinions expressed in this column are those of the author and do not represent those of Adhesives & Sealants Industry, its staff, Editorial Advisory Board or BNP Media.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

Recent Articles by Dave Dunn

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI May 2015 cover

2015 May

You won't want to miss our May issue, with a special packaging-focused Adhesives at Work section, as well as coverage of pressure-sensitive adhesives (PSAs), biorenewable feedstocks, and more!

Table Of Contents Subscribe

Better Jobs

Is the economy prompting you to consider leaving your job for a better one?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.