Focus On: Restoring History

May 1, 2012
Trans

PPG’s Protective and Marine Coatings business receives award for coatings performance on the restoration of the U.S. Capitol Dome.

PPG Industries recently announced its Protective and Marine Coatings business (PPG-PMC) has received the Society for Protective Coatings (SSPC) 2012 George Campbell Award. The honor recognizes the performance of PPG-PMC’s spot primer and finish coatings used in the restoration of the U.S. Capitol Dome in Washington, D.C.

The renovation project included two 100%-acrylic, waterborne enamel coatings from PPG—PITT-TECH® exterior spot primer and Pitt-Tech exterior finish DTM (direct-to-metal) satin industrial enamel, which was tinted to color-match the dome.

“It was an honor for PPG and me personally to be involved in a project that will be protecting one of the most recognizable buildings in the world,” said Todd DeBarba, technical sales representative, Protective and Marine Coatings, Northeast and Mid-Atlantic regions.

The George Campbell Award honors outstanding achievement in the completion of a difficult or complex industrial or commercial coatings project. Because the U.S. Capitol Dome was originally constructed in the 1790s, and due to its unique structure, this restoration project required detailed planning and precise execution throughout multiple phases. Also, because of the Capitol Dome’s historic significance and status as a popular tourist attraction, all access points and staging areas around the project had to be meticulously maintained by the restoration crew.

Also honored were the Architect of the Capitol, which is charged by the U.S. Congress with upkeep of the Capitol grounds and other landmarks in Washington, D.C., and Aulson Company, Methuen,MA, a specialty contractor that removed 100 tons of 140-year-old, lead-based paint from the Capitol Dome and then applied 700 gal of new paint.

About PPG

PPG Industries strives to continue to be the world’s leading coatings and specialty products company. Through leadership in innovation, sustainability and color, PPG helps customers in industrial, transportation, consumer products, and construction markets and aftermarkets to enhance more surfaces in more ways than does any other company. Founded in 1883, PPG has global headquarters in Pittsburgh and operates in more than 60 countries around the world. Sales in 2011 were $14.9 billion.

For more information, phone (888) 9PPG-PMC (977-4762) or visit www.ppgpmc.com/northamerica.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI April 2015 cover

2015 April

Our April issue includes previews of the ASC Spring Convention and Expo and the European Coatings Congress and Show, as well as articles detailing end-use applications in transportation, raw materials and equipment. Check it out today!

Table Of Contents Subscribe

Paid Leave

President Obama recently announced he wants U.S. businesses and the federal government to provide paid sick leave and paid parental leave to all workers. Do you think this is a good idea?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.