FDD6919 is a new resilient label optimized for laser and impact printing. Reportedly ideal for chemical drum labeling, the label can offer high strength, tear resistance, dimensional stability and temperature endurance. Available in a top-coated matte finish, it reportedly offers improved printability for laser and impact printing for a variety of durable label applications, including lawn and garden equipment, appliances, nameplates, and more.
FDD6919 is a 2-mil white polyester available with MP690 durable adhesives and a 3.4-mil C1S layflat liner. It has passed the British Maritime Standard BS 5609, a specification for printed pressure-sensitive, adhesive-coated labels for marine use that requires the label withstand a three-month saltwater submersion test.
For additional information, visit www.mactac.com.