Trans

Pipercross needed to update and improve existing resin mixing, dispensing, and automation processes.
 
Pipercross designs and manufactures air, oil and fuel filters for buses, trucks, and trains, as well as high-performance competition cars and super bikes. With over 28 years of experience in developing products for road and race applications, the company is at the forefront of filter technology. To continue to improve product performance, Pipercross realized it needed to update and improve existing resin mixing, dispensing, and automation processes. The company approached Liquid Control Ltd., a recent acquisition by Fisnar Inc., for assistance.
 

Necessary Improvements

Pipercross needed to bond and seal both ends of a filter element to ensure process integrity. To achieve a quality bond, it was necessary to accurately meter and mix a two-part component polyurethane and then dispense it into a rectangular or square mold. Dispense accuracy was vital to the quality of the filter, as inconsistencies would impair effectiveness. Excess material would potentially contaminate the active filter area, and too little material would increase the probability of a leak with subsequent rejection during test and inspection.
 
Ensuring repeatable viscosity of the mixed resin was also crucial to filter quality. This requirement is a function of accurate ratio metering and temperature control. Both conditions require constant, closed-loop and self-correcting flow control monitoring. The material wicking capability would be adversely effected should the viscosity vary, which would reduce the performance of the filter. Liquid Control’s equipment enabled Pipercross to improve filter production by accurately controlling dispense quantity and quality.
 

Efficient Process

An XYZ Cartesian robot is used in the automation of the manufacturing process. In the first step, the filter base is positioned on the robot, and a control function initiates the dispense cycle of the Liquid Control model DXE60 metering and mixing system. The remote mixing head and static mixer is mounted on the robot and precisely dispenses the mixed resin as the head follows the profile of the mold. This automatic process ensures accurate resin placement to accept a filter element during the next stage of the process.
 
After the base filter element is inserted into the mold, the partial assembly is presented to a temperature-controlled carousel for the polyurethane resin to cure. Once the base filter cure process is complete, the top mold is placed on the robot and the dispensing cycle repeated. Finally, the bonded filter base assembly is inserted into the top mold and the cure process is repeated. The completed process results in a final filter assembly with a polyurethane top and base mold.
 
“Because of the programmable control and dispensing precision of the DXE60, we were able to refine and improve the quality of our filters,” said Adam Hughes, design engineer with Pipercross. “In addition, we experienced a significant cost saving in our reject rate of 50%. Taking into account a 40% increase in production due to an increase in speed and critical improvements in reliability, we are a very happy Liquid Control customer.”
 
For more information, contact Fisnar Inc. at 15 Corporate Dr., Wayne, NJ 07474; phone (973) 646-5044; email info@fisnar.com; or visit www.fisnar.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI May 2015 cover

2015 May

You won't want to miss our May issue, with a special packaging-focused Adhesives at Work section, as well as coverage of pressure-sensitive adhesives (PSAs), biorenewable feedstocks, and more!

Table Of Contents Subscribe

Better Jobs

Is the economy prompting you to consider leaving your job for a better one?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.