MOMENTIVE: Epoxy System for Composites

This company recently unveiled a new epoxy system to hasten mass production of carbon-fiber composites for lightweight automotive structural components. Curing in as little as two minutes, the low-viscosity EPIKOTE™ resin 05475 and EPIKURE™ curing agent 05500 system can facilitate industrial scale high- or low-pressure RTM, with direct infusion of carbon fibers. 

Features and benefits of the new system include: a very low viscosity at the recommended injection and cure temperature of 115–120°C, and a long injection window of about one minute. The system can provide a solution for the production of structural composite parts in a shorter cycle time.

For additional information, visit www.momentive.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40