Coatings / New Products / Raw Materials and Chemicals

DOW CORNING: Resin

Dow Corning® 3055 resin reportedly allows manufacturers of high-performance coatings to formulate low-VOC, next-generation polysiloxane coatings with urethane, epoxy, polyester, alkyd, amine and acrylic systems utilizing amine functionality. Unlike moisture-cured polysiloxanes, the resin does not require titanate/tin catalysts or ambient moisture to cure. As a result, it does not contribute to volatile byproducts that can cause film stress and adhesion loss.

Polysiloxane hybrid coatings formulated with the resin reportedly exhibited long-term flexibility and improved chemical, thermal, UV, corrosion, and moisture resistance compared to epoxy and two-component polyurethane systems. In addition, adding the resin can improve the chemical resistance and flexibility of polysiloxane coatings beyond that of a traditional epoxy topcoat.

For additional information, visit www.dowcorning.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40