For as long as polyester chemistry has been used to produce composite parts, manufacturers have needed various paste consistency resin products to work in conjunction with the laminating process. These paste materials are often used for wet-on-wet and post-assembly requirements. Paste materials take advantage of similar chemistries to co-cure and have been tailored for consistency, cure rate, hardness, and a host of features focused on meeting specific performance needs.

VERSATILITY

Polyester-based bonding compounds offer unique advantages in certain requirements. While other chemistries may not be adjustable, polyester-based bonding

Polyester-based bonding compounds offer unique advantages in certain requirements. 

compounds use the same chemistry as the composites being fabricated, so the cure speed may be tailored around local temperatures. In most cases, putties can be adjusted for gel time and exotherm by manipulating the initiator (often called the catalyst) level and initiator type. In extreme cases, where ambient temperatures run as low 65°F or as high as more than 100°F, putty fabricators can offer seasonally adjusted versions of the same product.

Polyester chemistry is versatile and offers a broad range of base resins, including orthopthalic, isopthalic, dicyclopentadiene and vinyl esters. Each variety of resin offers unique performance characteristics. Putty formulas are not only tailored around cure speed, but also around flexibility, tensile, moisture resistance, shrinkage, color, sanding and other features. Many companies that offer resins also have an in-depth selection of putty products to solve fabrication needs.

PROCESSING

Polyester putties and adhesive materials are easy to process. Keep in mind that there is an advantage to the operators being familiar with the chemistry. Less training is required when an operator is comfortable with compatible lamination products; the same initiators are often used for both laminating and putty application. Equipment used for bulk requirements has the same advantage; the same style of equipment and supplier may be used to support both applications, thereby easing maintenance and equipment training.

In addition, product support for putty products is generally excellent, and these products are largely manufactured by the same companies that offer composite resins. Local representatives who are already visiting customers can provide a great deal of product depth and experience to composite assembly requirements.

Specific processes such as core installation, hull and deck assembly, and component bonding have a long history of time-proven success. Within the industry, a number of well-known articles, publications, application guides and manuals have been produced by various suppliers. The depth of information regarding materials—and, accordingly, the processes to apply these materials—is impressive. When discussing application requirements with vendors, be sure to ask if they have application support information for your requirements.

ON THE MARKET

The economy of polyester bonding is easy to understand. Polyester pricing is well-known within the composites industry. As a result of its chemical nature, polyester bonding often offers a cost advantage over nearly any other product available.

Innovative processes have led to an updated array of products to stay in step with fabrication technologies.

  • Some of today’s putty products can co-cure within closed tooling processes.
  • Double-sided tooling requires a putty to gap fill and bond, such as with in-mold displacement (IMD).
  • Bonding putties are available for spray as well as extrudable applications.
  • Vehicle fabrication requires bonding putties with low shrink and print to suit demanding surface finish.
  • Other new products include bonding and filling putties that are fire retardant, smoke suppressive and low in toxicity.

Applications for bonding putties have expanded exponentially to cover ever-changing requirements. Today, specialty putty products have expanded roles beyond bonding, filling and fairing. Specialty products are used for combination requirements, such as radius filling and print blockage, and some polyester putty products can edge-fill and reinforce honeycomb cores. In addition, putty products are now available as routable material to fabricate master patterns for tooling.

Polyester bonding materials are not a panacea, but they do deserve a first look. The versatile chemistry offers easy processing, product support, range of materials and obvious economy. Industry demands that manufacturers consider the best options for bonding requirements, and this assembly solution should remain at the forefront for fiberglass fabrication.


For more information, contact the author at (819) 477-1180 or murray.akerman@ccpcomposites.ca.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI February 2015 cover

2015 February

You won't want to miss our special Adhesives at Work: Electronics section, plus articles on converting/packaging, silicones, coatings and more!

Table Of Contents Subscribe

Paid Leave

President Obama recently announced he wants U.S. businesses and the federal government to provide paid sick leave and paid parental leave to all workers. Do you think this is a good idea?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.