Hernon Manufacturing recently announced it was given approval for its Dripstop® 940 anaerobic pipe sealant from TerraCair, a manufacturer of diesel exhaust fluid (DEF) and urea. DEF is used with the catalytic converters for diesel engines made since 2010.

TerraCair publishes and distributes a DEF Equipment Suppliers list of approved companies that they have found to be contaminant-free and compliant with proper usage of DEF. Dripstop 940 was approved as a suitable pipe sealant for DEF technology and is now included on the list.

“As a result of a meeting with TerraCair representatives at the Petroleum Equipment Institute (PEI) show last month, Hernon Manufacturing was given the proper direction and contacts to pursue the listing,” said Bob Sollien, Northeast sales representative for Hernon Manufacturing.

The sealant also received the necessary approvals and exhibited 100% passing results from Intertek, which conducts thousands of automotive fuel and lubricant analytical tests each month. This testing confirmed that Dripstop 940 was containment free to ISO-22241 standards and therefore compatible for DEF technology.

For additional information, visit www.hernon-defsystems.com

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

In-Depth Features

These articles detail advantages and innovations for multiple end uses.

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI April 2014 cover

2014 April

Our April issue focuses on pressure-sensitive adhesives, including a preview of PSTC's 2014 Tape Summit, as well as converting/packaging and composites!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40