Zircotec Develops Heatshield Coating

Zircotec recently announced it can offer a specific coating or heatshield tailored to the needs of engineers. ThermoHold® GOLD (for composites) and ZircoFlex® GOLD reportedly provide protection from both conductive and radiant heat sources due to a blend of ceramic insulation and real 24 carat gold, providing 98% reflectivity.

Research conducted by Zircotec on existing “gold” heatshields reportedly found that many did not actually contain gold; these were simply aesthetic finishes with no real improvement in heat reflectivity. Many products were copper-based and, while they were effective when new, the copper quickly oxidized when temperatures exceed 500°C, reducing its ability to reflect heat away. Furthermore, neither of the products tested offered any real protection from conductive heat.

“The reflective properties of gold have long been trusted to protect sensitive components against heat,” said Terry Graham, managing director. “However, real gold foil is rarely used; it is highly expensive and offers little or no protection against conducted heat. Our new products enable engineers to manage both forms of heat with a single gold finished coating or ZircoFlex GOLD heatshield product, thereby helping to solve packaging and installation issues.”

ZircoFlex GOLD heatshield is 0.17 mm thick and, at 230 g/m², is half the weight of the current ZircoFlex product. Combining superlight weight with its ability to be cut and folded reportedly allows it to be used for weight-sensitive or package-restricted applications such as Formula One, high-end motorsport, aerospace, or defense.

For additional information, visit www.zircotec.com

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI June 2013 cover

2013 June

The 2013 June Adhesives and Sealants Industry Magazine includes articles about Nordson EFD and UV curing with lasers, as well as a case study on progressive cavity pumps. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40