Zircotec Develops Heatshield Coating

Zircotec recently announced it can offer a specific coating or heatshield tailored to the needs of engineers. ThermoHold® GOLD (for composites) and ZircoFlex® GOLD reportedly provide protection from both conductive and radiant heat sources due to a blend of ceramic insulation and real 24 carat gold, providing 98% reflectivity.

Research conducted by Zircotec on existing “gold” heatshields reportedly found that many did not actually contain gold; these were simply aesthetic finishes with no real improvement in heat reflectivity. Many products were copper-based and, while they were effective when new, the copper quickly oxidized when temperatures exceed 500°C, reducing its ability to reflect heat away. Furthermore, neither of the products tested offered any real protection from conductive heat.

“The reflective properties of gold have long been trusted to protect sensitive components against heat,” said Terry Graham, managing director. “However, real gold foil is rarely used; it is highly expensive and offers little or no protection against conducted heat. Our new products enable engineers to manage both forms of heat with a single gold finished coating or ZircoFlex GOLD heatshield product, thereby helping to solve packaging and installation issues.”

ZircoFlex GOLD heatshield is 0.17 mm thick and, at 230 g/m², is half the weight of the current ZircoFlex product. Combining superlight weight with its ability to be cut and folded reportedly allows it to be used for weight-sensitive or package-restricted applications such as Formula One, high-end motorsport, aerospace, or defense.

For additional information, visit www.zircotec.com

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI May 2015 cover

2015 May

You won't want to miss our May issue, with a special packaging-focused Adhesives at Work section, as well as coverage of pressure-sensitive adhesives (PSAs), biorenewable feedstocks, and more!

Table Of Contents Subscribe

Better Jobs

Is the economy prompting you to consider leaving your job for a better one?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.