OMNOVA SOLUTIONS: Colloidal Dispersion

PLIOTEC® SA60 is a new colloidal dispersion fortified with a water-based epoxy to form a 2K coating system. This system can reportedly be used on interior vertical walls in institutional locations such as schools, hospitals, warehouses, office buildings, correctional facilities and other high traffic areas that are subject to frequent cleaning.

PLIOTEC SA60 can reportedly be formulated into a protective coating that has high abrasion and scuff resistance and is resistant to strong cleaning products. Low VOC, low odor, APE free, excellent adhesion and fast drying are all attributes of institutional coatings formulated with the material.

For additional information, visit www.omnova.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40