7833 PET is a new elevated-temperature acrylic adhesive transfer tape on a PET film liner for thermoforming in aerospace, automotive, appliance, electronic and medical applications. The 1.5-mil PET liner product carries a 3-mil pressure-sensitive acrylic adhesive with a biostatic additive for mold control. It can be used in applications with intermittent temperatures to 300ºF.

The tape can be pre-applied to thermoformable materials, reportedly permitting forming to mild contours and eliminating post-forming adhesive application to finished parts. It is available at 49 in. wide.

For additional information, visit www.adchem.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI June 2013 cover

2013 June

The 2013 June Adhesives and Sealants Industry Magazine includes articles about Nordson EFD and UV curing with lasers, as well as a case study on progressive cavity pumps. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40