Ultra Light-Weld® 431 is reportedly a versatile adhesive for glass-to-glass and glass-to-metal applications. The product has been formulated to be resistant to
high-temperature and high-moisture environments while maintaining adhesion and flexibility. It was also designed with low shrinkage, which can reduce stress on the bond line or on larger cured surfaces.
The adhesive can bond rapidly upon exposure to UV/visible light for immediate use in the assembly process. Applications include assembly (e.g., furniture), container glass, and lighting and appliance sub-assemblies. The adhesive is designed for bonding glass and metal, but can also be considered for bonding a variety of plastics, as well as ceramic and FR4.