Advancing Adhesives: Water-Based Polyurethane Goes Green

Soy oil replaces petroleum in water-based polyurethane coatings and adhesives.

March 1, 2013
Trans

Battelle scientists have reportedly invented a novel, water-based polyurethane unlike any other—environmentally responsible, cost-effective, soy-based and free of N-methyl-2-pyrrolidone (NMP) solvent. This new polyurethane has less odor than its petroleum-based counterpart and can be used in a variety of coatings and adhesives.

The product can prove to be environmentally superior on two levels. It uses soy oil instead of petroleum to produce the polyol needed to make standard polyurethanes. In addition, water-based polyurethanes must have NMP added during the manufacturing process in order to lower viscosity. This proprietary formulation eliminates the need for that expensive solvent, a breakthrough that can reduce costs, handling, reporting regulations, vapors, and pollution.

The polyurethane is a product of research fostered in Battelle’s formal mentoring program. It was funded by Ohio soybean farmers through the Ohio Soybean Council (OSC).

“Once again, our friends at Battelle have developed a remarkable new product that takes advantage of the versatility of soybean oil,” said Keith Roberts, OSC New Uses Committee chair and soybean farmer from Marion County, Ohio. “Our investment in research to develop new products made from renewable, environmentally friendly soybeans benefits everyone, including Ohio and all U.S. soybean farmers.”

Both proof-of-principle and lab-scale testing were established at Battelle; Ram Lalgudi, senior research scientist, presented a paper on the subject at conferences in 2012. Lalgudi mentored Researcher Phil Denen, a young scientist at Battelle who started the idea and worked on weekends and off-work hours to develop it. Battelle has intellectual property based on the product and has filed for a patent.

“Yes, this new product is important for the consumer because it’s environmentally friendly and does the same job at a comparable price as older polyurethanes without using volatile organic solvents such as NMP,” said Rick Heggs, senior Marketing manager at Battelle. “But for manufacturers, this represents a leap forward. Eliminating NMP makes life a lot easier.”

Applications for the new product include all kinds of paints, inks, top coatings, and seal coatings, and will also be valuable in the peel-and-go market and a variety of adhesives. It meets Chemical Agent Resistant Coatings (CARC) standards, which means it will be usable by the military. Battelle will reportedly seek licensing partners to scale up the product to mass manufacturing.


ABOUT BATTELLE
Reportedly the world’s largest independent research and development organization, Battelle provides innovative solutions to the world’s most pressing needs. It advances scientific discovery and application by conducting $6.5 billion in global R&D annually through contract research, laboratory management and technology commercialization. Headquartered in Columbus, Ohio, Battelle oversees 22,000 employees in more than 130 locations worldwide, including eight national laboratories for which Battelle has a significant management role on behalf of the U.S. Department of Energy, the U.S. Department of Homeland Security, and the UK. For more information, visit http://battelle.org.
 

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI April 2015 cover

2015 April

Our April issue includes previews of the ASC Spring Convention and Expo and the European Coatings Congress and Show, as well as articles detailing end-use applications in transportation, raw materials and equipment. Check it out today!

Table Of Contents Subscribe

Better Jobs

Is the economy prompting you to consider leaving your job for a better one?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.