Can you offer some advice regarding the sourcing of monomers for acrylic adhesives formulations?

QUESTION: We are formulating acrylic adhesives (both reactive acrylics and anaerobics), but are having problems with the sourcing of monomers. Some suppliers can’t seem to give us monomers that produce shelf-stable products, even though they purport to have added extra free-radical stabilizers. Can you offer some advice?

ANSWER: These types of adhesives can be quite complicated to formulate. Without knowing the specifics of your formulation, I can only suggest the following: in addition to the polymerizable monomers and other additives, two major factors influence the reactivity of these adhesives: initiators/accelerators and stabilizers.

Initiators and accelerators are usually hydroperoxides and aromatic amines. When the applied adhesives come in contact with metallic surfaces like iron or copper, these initiation systems generate free radicals, which polymerize the monomers to give cured products. Stabilizers, on the other hand, come in two types. The first type of stabilizer, atmospheric oxygen, is a strong free-radical stabilizer. As a result, these adhesives are often packaged in thin containers made of low-density polyethylene that allow the air to permeate the package.

Secondly, extra stabilizers such as quinones are added to give additional shelf stability. In your case, it seems that the extra stabilizers are not giving the desired stability. I would suggest that you look at the strong possibility that the monomers contain traces of iron or copper, perhaps residues from your supplier’s manufacturing equipment. Traces of these metals are the real enemy of the anaerobic adhesives formulator, and you should ask your suppliers to remove them or complex them with a metal chelator. You can also add a metal chelator to your formulation, but be careful about not adding too much and affecting your cure speed. 


Any views or opinions expressed in this column are those of the author and do not represent those of Adhesives & Sealants Industry, its staff, Editorial Advisory Board or BNP Media.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

Recent Articles by Dave Dunn

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI April 2015 cover

2015 April

Our April issue includes previews of the ASC Spring Convention and Expo and the European Coatings Congress and Show, as well as articles detailing end-use applications in transportation, raw materials and equipment. Check it out today!

Table Of Contents Subscribe

Better Jobs

Is the economy prompting you to consider leaving your job for a better one?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.