Composites / Manufacturers / Finished Adhesives and Sealants

Case Study: Passing the Torch

The London 2012 Olympics opening ceremony powerboat was fabricated using structural adhesives.

April 9, 2013
Trans

The now world-famous powerboat that was driven up the Thames by David Beckham to bring the Olympic flame to the London 2012 Olympics opening ceremony was a Bladerunner BR RIB 35. This unique British fiberglass powerboat was designed and manufactured by ICE Marine Ltd. and fabricated using Scott Bader Crystic® products. The craft’s heritage and racing design pedigree comes from Lorne Campbell, ICE Marine’s chief naval architect, and the 1995 two-liter Powerboat World Champion and Managing Director Jeremy Watts, who was also the Bladerunner driver during the torch handover part of the opening ceremony event.

Functionality and Form

Bladerunner powerboats are individually handbuilt to order by ICE Marine’s production team. They use both open-mold hand lay-up and vacuum bagging processes. The Bladerunner BR RIB35 laminate design uses a Lloyd’s-approved, Scott-Bader-matched marine system comprised of pigmented Crystic 65PA isophthalic gelcoats combined with Crystic 489PA isophthalic unsaturated polyester back-up resin.

ICE Marine has been using Crystic resins and gelcoats to make its high-performance powerboats for over 14 years. “We have been very impressed with the quality and performance reliability of Scott Bader products, which are also easy to use on the shop floor as they have excellent batch-to-batch consistency,” says Watts. “We know what we are getting every time.”

Depending on the Bladerunner model and specification required by a customer, laminate constructions use a combination of chopped strand matting, biaxial and unidirectional glass and carbon fiber fabrics, as well as DIAB’s Divinycell H80 and H100 PVC foam cores. Sandwich laminate sections are used extensively in the structural design of both the hull and deck.

Product Performance

Reliable product performance on the water in line with the demanding design specifications of a Bladerunner BR RIB 35 powerboat is critical. Fitted with either a 300- or 350-hp supercharged Mercury Verado outboard gasoline engine, speeds of up to 72-77 knots (82-88 mph) can be achieved, putting enormous pressure on the hull at top speed.

To achieve the highest long-term mechanical performance of the laminate sandwich structures in key stress areas, PVC foam cores are first primed using a light coating of catalyzed Crystic 489PA resin and then bonded in with Crystic Crestomer 1196PA, a low-density, gap-filling structural adhesive specially designed for core bonding. Vacuum bagging is used by ICE Marine, as recommended by Scott Bader, to ensure void-free adhesion and to maximize the penetration of the gap-filling structural adhesive around the PVC core material. The core bonding performance of Crestomer 1196PA has been well proven for many years by many other leading fiberglass boat builders, who also value the added benefit of improved hull and deck surface finish and reduced print-through by using Crestomer 1196PA for core bonding.

 The Bladerunner series is founded on the desire to build a highly efficient, offshore-performance-focused powerboat that is able to offer significantly improved ride comfort and handling in open water at speed. This has been achieved by ICE Marine with its innovative “double-scoop” air entrapment monohull (AEM) design, which is used for all Bladerunner powerboats. This AEM monohull design was co-developed by Watts and Lorne Campbell, who has 30 years’ experience as a naval architect designing class-winning, high-performance powerboats and trimarans. Campbell’s designs have 100 race wins and 20 world and national championships.  


 

About Scott Bader

Scott Bader was established in 1921. Today it is a $300 million multinational polymers company employing 600 people worldwide. It is a common trusteeship company, having no external shareholders, with a strong commitment to support its customers, workforce and the environment. Based in the UK, the company’s purpose-built, state-of-the-art technical facilities provide R&D as well as complete evaluation, testing and application support. The company has manufacturing facilities in the UK, France, Croatia, the Middle East and South Africa. For additional information, call (44) 1933-663100, email info@scottbader.com, or visit www.scottbader.com or www.scottbaderinc.com


For more information about ICE Marine Ltd., visit www.icemarine.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI April 2015 cover

2015 April

Our April issue includes previews of the ASC Spring Convention and Expo and the European Coatings Congress and Show, as well as articles detailing end-use applications in transportation, raw materials and equipment. Check it out today!

Table Of Contents Subscribe

Better Jobs

Is the economy prompting you to consider leaving your job for a better one?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.