Advancing Adhesives: Mussels Inspire Innovative New Adhesive for Surgery

A new synthetic family of adhesives can serve as bioadhesives.

Mussels can be a delicious meal, but the chemistry that lets mussels stick to underwater surfaces may also provide a highly adhesive wound closure and more effective healing from surgery. In recent decades, bioadhesives, tissue sealants and hemostatic agents became the favored products to control bleeding and promote tissue healing after surgery. However, many of them have side effects or other problems, including an inability to perform well on wet tissue.

“To solve this medical problem, we looked at nature,” said Jian Yang, associate professor of bioengineering at Penn State. “There are sea creatures, like the mussel, that can stick on rocks and on ships in the ocean. They can hold on tightly without getting flushed away by the waves because the mussel can make a very powerful adhesive protein. We looked at the chemical structure of that kind of adhesive protein.”

Yang, along with University of Texas-Arlington researchers Mohammadreza Mehdizadeh, Hong Weng, Dipendra Gyawali and Liping Tang, took the biological information and developed a wholly synthetic family of adhesives. They incorporated the chemical structure from the mussel’s adhesive protein into the design of an injectable synthetic polymer. The bioadhesives, called iCMBAs, adhere well in wet environments, have controlled degradability, improved biocompatibility and lower manufacturing costs, putting them a step above current products such as fibrin glue and cyanoacrylate adhesives.

Fibrin glues are fast acting and biodegradable but have relatively poor adhesion strength. They may also carry the risk of blood-borne disease transmission and have the potential for allergic reactions due to animal-based ingredients. Cyanoacrylate adhesives offer strong adhesion, rapid setting time and strong adhesion to tissue, but they degrade slowly and may cause toxicity, often limiting their use to external applications. In addition, neither product is effective when used on wet tissue, a requirement of internal organ surgery, nor are there any current commercially available tissue adhesives or sealants appropriate for both external and internal use.

The researchers tested the newly developed iCMBAs on rats, using the adhesive and finger clamping to close three wounds for two minutes. Three other wounds were closed using sutures. The researchers reported their findings in a recent issue of Biomaterials.1

The iCMBAs provided 2.5 to 8.0 times stronger adhesion in wet tissue conditions compared to fibrin glue. They also stopped bleeding instantly, facilitated wound healing, closed wounds without the use of sutures and offered controllable degradation.

“If you want the material to stay there for one week, we can control the polymer to degrade in one week,” said Yang. “If you want the material to stay in the wound for more than a month, we can control the synthesis to make the materials degrade in one month.”

The iCMBAs are also non-toxic, and because they are fully synthetic, they are unlikely to cause allergic reactions. Side effects were limited to mild inflammation. “If you put any synthetic materials into your body, the body will generate some inflammation,” Yang said.

The researchers are now working on improving the formula. “We are still optimizing our formulation,” he said. “We are trying to make the adhesion strength even stronger” to expand its use for things like broken bones where strong adhesion is tremendously important. The researchers are also looking at adding components that could control infection.

“We can introduce another component with anti-microbial properties, so it can do two functions at once,” said Yang.

The iCMBAs could eventually be used in a wide range of surgical disciplines from suture and staple replacement to tissue grafts to treat hernias, ulcers and burns. “There are so many applications that you can use this glue for to help in surgery,” he said.


For more information, visit www.psu.edu.


Reference

 1. Mehdizadeh, Mohammadreza, Weng, Hong, Gyawali, Dipendra, Tang, Liping, Yang, Jian, “Injectable Citrate-Based Mussel-Inspired Tissue Bioadhesives with High Wet Strength for Sutureless Wound Closure,” Biomaterials, 2012; 33 (32): 7972. 


 

To find suppliers of raw materials and chemicals, as well as other products, visit www.adhesivesmag.com/suppliers.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI June 2015 cover

2015 June

Welcome to our annual Dispensing & Curing Equipment Directory!
Table Of Contents Subscribe

"Cultural Fit"

A recent opinion piece in the New York Times observed that new employees are often hired based on the personal similarities they share with their interviewers. How important is “cultural fit” when hiring someone?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.