Carbon Nanotube-Based Coatings

New coatings containing CNTs offer enhanced strength and corrosion resistance.

May 1, 2013
Trans

Carbon nanotubes (CNTs) are nanometer-scale tubular structures consisting entirely of carbon atoms (see Figure 1). They represent a newly discovered elemental form of carbon and have remarkable properties in terms of mechanical strength, thermal conductance and electrical conductivity. CNTs are the strongest materials ever discovered, with tensile strengths reported to be 50 times that of steel. They can also have conductivities 1,000 times that of copper.

Since their discovery, CNTs have been an intense focus area in nanotechnology research. Advancements in synthesis technologies have now allowed for the large-scale production of CNTs such that these materials are finding their way into commercial product applications.

CNTs are available in a variety of forms, including single-walled nanotubes (SWNTs) and multi-walled nanotubes (MWNTs). In addition, MWNTs can be produced having a “Russian doll” structure consisting of individual tubes within tubes, or having a “parchment” structure consisting of a continuous, multi-rolled sheet of carbon. CNTs can also come in a variety of chiralities based on how the sheet of carbon atoms are connected together (including so-called “zig-zag” and “armchair” configurations), as well as in a range of different sizes, with typical diameters of 1-3 nm and lengths that approach several microns (with aspect ratios exceeding 1,000x).

Different types of CNTs can exhibit large differences in terms of strength, conductivity and other properties. Commercially available CNTs normally consist of complex mixtures of tube types and sizes, thus making proper CNT selection a critical requirement for successful results in a given application.

Use of Carbon Nanotubes in Corrosion-Control Coatings

A new series of corrosion-control coatings containing CNTs is now being developed and made available for end-user sampling. These coatings have enhanced strength and electrical conductivity due to the inclusion of CNTs, while also incorporating sacrificial metal particles (e.g., Zn, Al, Mg) for corrosion inhibition via cathodic protection. These coatings can be applied using standard painting equipment (conventional and HVLP air spray, airless spray, brush, roller, etc.) and are based on traditional coating polymers, including epoxy and urethane chemistries. CNTs allow sacrificial metal-filled primers to be formulated at much reduced metal content vs. traditional systems.

Although epoxy primers filled with zinc dust (e.g., MIL-PRF-24441/19) have been widely used for heavy-duty industrial maintenance applications for many years, these primers (also known as zinc-rich primers) must be formulated with very high levels of zinc dust (80-90% wt) to ensure point-to-point contact of zinc particles and effective galvanic activity (see Figure 2). As such, these coatings can be brittle/porous and exhibit poor substrate and/or inter-coat adhesion due to the binder-starved condition of the coating film. The application of an intermediate coating is normally required to stabilize the primer film before topcoat application.

Alternatively, in a CNT/Zn-based epoxy primer, CNTs are used to establish conductive pathways within a coating film so that lower levels of zinc metal are required (see Figure 3). This results in a tougher, more binder-rich primer film that exhibits better flexibility and adhesion. An intermediate coating is not required before final topcoat application. The use of a two-coat, CNT-based system can thus provide considerable project cost/time savings vs. conventional three-coat systems.

The establishment of conductive networks in the coating film occurs due to the unique ability of carbon nanotubes to bond together and form rope-like structures. Strong van der Waals interactions occur between CNTs. They can also bond together covalently through a process known as p-stacking.

Field Testing of CNT/Epoxy Zinc-Rich Coatings

In 2009, a CNT-based epoxy primer containing zinc dust was demonstrated in a field trial with the U.S. Army Corp of Engineers at Fort Bragg, N.C. In this project, a CNT/Zn-based epoxy primer/urethane coating system was applied to the exterior of a steel storage tank that was suffering from corrosion damage.

The existing coating, a conventional three-coat zinc-rich epoxy/epoxy intermediate/urethane topcoat system, was removed with abrasive blasting to SSPC SP10 near-white metal specifications, followed by the application of the two-coat CNT-based system. Extended immersion, salt-fog and outdoor fence testing of the coatings was also conducted. Results have been excellent, and the U.S. Army Corp is considering possible implementation of the coatings as a replacement for the traditional three-coat, mil-spec systems.

A Technology Platform for Advanced Coatings

The excellent results obtained with CNT/Zn-based systems during field and laboratory testing with the U.S. Army Corp show that these coatings may offer an important technology platform for enhanced corrosion-protective systems in other coating applications beyond the atmospheric protection of steel substrates. For example, other types of coatings can be developed and tailored for different applications through the careful selection of CNT types, polymer chemistries, and sacrificial metal choice.

For example, research is now being conducted on CNT-based coatings containing sacrificial magnesium pigments for the protection of aluminum substrates in aerospace applications. Magnesium can provide cathodic protection to aluminum in the same way that zinc provides protection to steel, and significantly reduced levels of magnesium are needed when conductive CNTs are incorporated.

Current aerospace primers rely on a passivating mechanism to control corrosion by incorporating hexavalent chromate pigments that are highly carcinogenic and environmentally unsafe. A CNT-based coating using sacrificial magnesium would operate by a completely different mechanism and would not require chromate pigments. Hazardous pretreatment processes could be potentially eliminated as well.

Given the severity of corrosion problems in the U.S. and abroad, and the need for improved coatings, CNT-based coatings for corrosion-control applications should generate significant interest within the industry. The direct annual costs of corrosion in the U.S. are over $400 billion per year, and CNT-based coatings may represent an important new technology to help reduce costs.


 For additional information, visit www.teslanano.com

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI march 2015 cover

2015 March

Welcome to our annual Raw Materials, Chemicals, Polymers and Additives Handbook!
Table Of Contents Subscribe

Paid Leave

President Obama recently announced he wants U.S. businesses and the federal government to provide paid sick leave and paid parental leave to all workers. Do you think this is a good idea?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.