This company’s new 6B23 (3 x 3 ml) dual syringe can be used with a variety of low-cost static mixers for meter-mix and dispensing of plural component epoxies, urethanes, or 1:1 ratio compositions. It can be used without a static mixer for hand-mix applications, and is available in ultra-clear polypropylene, opaque polyethylene or nylon material for chemical resistance.

The dual syringe product line includes 30-, 14-, 6- and 4-ml sizes that come in a 1:1 ratio. The 30-ml syringe is also available in a 2:1 ratio.


 For additional information, visit www.plaspakinc.com