Can you suggest ways to improve an adhesive system in terms of moisture/water sensitivity?

 QUESTION: We are successfully structurally bonding Belgian Blue Stone—also called Petit Granit (a non-porous limestone material)—with a two-component epoxy in an industrial process. Three-point bending tests have resulted in nearly 100% material (stone) failure. During recent long-term qualification tests, however, the system seemed to be moisture- and water-sensitive, resulting in adhesion failure and delamination of the glue. Can you suggest some improvements to the adhesive system?

ANSWER: Many epoxies are routinely used for applications where they are immersed for long periods (sometimes many years) in fresh or salt water. It may be helpful to ask your adhesive supplier for a more suitable product. On the other hand, if you are a formulator, then I would suggest using an organosilane additive at 1-2% in your product. Organosilanes act as “bridging” molecules between mineral surfaces and organic adhesives and prevent hydrolysis at the adhesive-substrate interface.

From an epoxy resin point of view, standard bisphenol-A diglycidyl ether (BADGE) epoxies are usually adequate for the application, but you should look closely at both the hardener component of your adhesive and the fillers. Some hardener components, such as certain polyamides, do not seem to survive long periods of water immersion. I have had considerable success using cycloaliphatic amines. Silica and mica fillers are useful for water-resistant properties.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

Recent Articles by Dave Dunn

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI march 2015 cover

2015 March

Welcome to our annual Raw Materials, Chemicals, Polymers and Additives Handbook!
Table Of Contents Subscribe

Paid Leave

President Obama recently announced he wants U.S. businesses and the federal government to provide paid sick leave and paid parental leave to all workers. Do you think this is a good idea?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.