BASF, Cargill and Novozymes recently announced an important milestone in their joint development of technologies to produce acrylic acid from renewable raw materials by successfully demonstrating the production of 3-hydroxypropionic acid (3-HP) in pilot scale. 3-HP is a renewable-based building block and one possible chemical precursor to acrylic acid.

The companies also have successfully established several technologies to dehydrate 3-HP to acrylic acid at lab scale. This step in the process is critical since it is the foundation for production of acrylic acid. In August 2012, BASF, Cargill and Novozymes announced their joint agreement to develop a process for the conversion of renewable raw materials into a 100% bio-based acrylic acid.

“3-HP is a potential key raw material for the production of bio-based acrylic acid, which is a precursor of superabsorbent polymers,” said Teressa Szelest, senior vice president, Global Hygiene business, BASF. “We still have a fair amount of work to do before the process is commercially ready, but this is a significant milestone and we are confident we can continue to the next level of scale-up for the entire process in 2014.”  

Acrylic acid is a high-volume chemical that feeds into a range of products. BASF is the world’s largest producer of acrylic acid and has substantial capabilities in its production and downstream processing. BASF reportedly plans initially to use the bio-based acrylic acid to manufacture superabsorbent polymers that can soak up large amounts of liquid and are used mainly in baby diapers and other hygiene products.

Superabsorbent polymers derived from bio-based acrylic acid are expected to be a groundbreaking new offer to the market. Diapers made of such superabsorbent polymers could meet the demand of a significant and growing group of consumers in mature markets in particular. They also may allow diaper producers to meet consumer demands, differentiate their products and contribute to their sustainability goals.

For additional information, visit www.novozymes.com, www.cargill.com or www.basf.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI July 2014 cover

2014 July

Our annual Distributor Directory helps you locate a distributor that best suits your needs. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px