Hardman aircraft sealants are manufactured at the company’s Wilmington, CA, facility, which has been certified to the AS 9100, ISO 9001/2000 and AS7200/1 NADCAP quality systems requirements and sold to aerospace and defense customers that require qualified sealants for demanding fuel tank and environmental sealing applications.
Royal CEO Ted Clark said, “This product qualification is a significant achievement for the company and underscores our efforts to listen to customers’ requirements for improving quality and reducing costs through sealants that cure 50% more rapidly than the current generation sealants. This allows for faster aircraft assembly and reduces the time for repair and maintenance, which will reduce our customers’ overall costs.”
AMS 8802-qualified aircraft sealants are used on virtually all U.S.-manufactured military aircraft. In addition to its rapid cure, WS 8020 RC exhibits outstanding resistance to aviation gasoline and jet fuel, as well as resistance to chemicals and petroleum products common to the aircraft industry. It also offers excellent flexibility and bond strength to most metal substrates, including aluminum, stainless steel, steel, advanced composites, and many coatings under extremes of temperature, weathering, and stress.
Hardman WS 8020 RC is a rapid-cure aircraft sealant qualified to Class B of the AMS 8802 sealant specifications. WS 8020 RC Class B-2 has a work life of two hours, but cures to 30 shore A in just 12 hours - a reduction of 12 hours over standard AMS 8802-qualified sealants that have a cure rate of 24 hours.
“The qualification of Hardman WS 8020 RC aircraft sealant to AMS 8802 will benefit all military aircraft manufacturers, as well as military maintenance operations,” said Jeff Swindells, product manager, Aerospace Sealants. “In addition, WS 8020 RC is either qualified or under qualification at a number of business jet manufacturers in the United States and Europe.”

High-performance adhesives, sealants, encapsulants, potting compounds and mirror mastics make up the Royal Adhesives & Sealants product mix. These high-performance products are used in a variety of markets including aerospace and defense, assembly, automotive and recreational vehicle, electrical/electronic, filter, marine, and general industrial. The company also offers a range of thermosetting epoxy and urethane, solvent-based, and water-based technologies to meet the most demanding adhesive and sealant applications.
About Royal Adhesives and Sealants LLC
Royal Adhesives and Sealants manufactures and markets industrial adhesives and sealants, commercial roofing adhesives, and mirror mastics. The company makes solvent- and water-based adhesives and sealants that are packaged in totes, drums, pails, cartridges, and foil-wrapped sausages.For more information, visit www.royaladhesives.com.


More