Pyro-Putty 1000 is an advanced, two-part, water-based, ceramic- and aluminum-filled paste that operates to 1400 degrees F. This product is now used to repair defects in cast aluminum manifolds, seal aluminum housings found in infrared ovens, bond-burner components in commercial stoves, and seal sheet metal exhaust stacks found in industrial furnaces and incinerators. Pyro-Putty 1000 is an easy-to-use, environmentally compliant compound containing no asbestos or volatile organic compounds. It is a two-part powder and liquid system that is typically mixed to a paste-like consistency then dispersed into place in cross-sections up to ½" thick. Pyro-Putty 1000 sets at room temperature in 16-24 hours and can be cured in-situ or by heating for 1-2 hours at 160 degrees F. Cured product exhibits minimal shrinkage and can be sanded to a smooth finish, then coated with conventional paints or powder coatings.

For more information, visit http://www.aremco.com or e-mail aremco@aremco.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40