Ashland and Flint Group Sign Distribution Agreement

Coatings and adhesives from Ashland Performance Materials, a commercial unit of Ashland Inc., that are marketed to North American narrow web label, tag, and wrapper converters will now also be available from Flint Group. Effective March 15, Ashland and Flint Group will begin a distribution and co-branding effort that calls for Flint Group to begin marketing Ashland products under a co-branded label that will carry the Flint Group trademark or trade name.

The long-term agreement enables Flint to distribute Ashland’s radiation-cure, water-based and solventless laminating adhesives and coatings in North America. Flint Group will also acquire the management of some Ashland customers and will provide them with dedicated sales, technical service, and customer service support.

“Flint Group is a world-class organization that brings a strong market presence to Ashland’s coatings and adhesive products,” said Kelly Williams, market development manager for Ashland’s Laminating Adhesives and Coatings. “Flint Group’s capabilities reach all of our key markets, and they bring top-notch commercial and technical staff with demonstrated abilities to grow business.”

“We were chosen due to our strength and stature in the printing industry,” said Susan Kuchta, vice president, North American Packaging and Narrow Web business, Flint Group. “We are proud of our broad offering and excellent customer support. This relationship adds other key products to our portfolio in order to better support package and label printers.”

For more information, visit www.ashland.com or www.flintgrp.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40