Ask Dr. Dave / Columns

Ask Dr. Dave

January 2005

QUESTION: Do solid sticks and gel threadlockers work as well as liquid versions?

ANSWER: Most people who use anaerobic threadlockers use liquids that come in the traditional red or blue tubes or bottles. These work fine for most applications, but the liquids have a tendency to drip and are quite tricky to use in certain situations, like overhead assembly applications. Both the stick and gel products overcome this weakness. The stick products come in a "propel" type container that looks just like an industrial Chap Stick container. This container is highly functional, can be operated using one hand and allows one to rub the product onto threads or to rotate the threaded component across the stick. The gel product is supplied in a distinctive "propel-repel" container with a nozzle and transparent cap. While this container can also be operated using one hand, it does require some practice. The real benefit of the gel product seems to be in treating difficult-to-reach threads, such as some studs and partially assembled fasteners, and also female threads where the nozzle really helps in applying the product. I have not tested the performance properties of the products, but information from the manufacturers indicates comparable performance to the liquid versions. I wouldn't hesitate to add both of these products to my toolbox.

QUESTION: We are constructing research water tanks that will include windows submerged from one side, but not under any significant pressure. Is there a suitable sealant to fix the glass pane to the steel frame? Is there a suitable sealant to fix the tank's steel frame into a concrete wall?

ANSWER: For attaching the glass pane to the steel frame, you might consider a high-performance RTV silicone. These products have been used in aquarium construction for many years. However, it is very important to have the correct joint design so that the silicone is acting mainly as a sealant and is not exposed to large stresses. You should also be sure to get a specific recommendation from one of the major silicone manufacturers, as only a few RTV silicones are suitable for this application.

For attaching the steel frame to a concrete wall, you might try a high-performance epoxy adhesive sealant or polysulphide sealant. A primer may be necessary for good adhesion; your supplier should be able to make a more specific recommendation.

Q&A Exchange is written by Dr. Dave Dunn of F.L.D.Enterprises, a technical consultancy and full-service industrial market research firm specializing in the adhesives, sealants, specialty rubbers, and plastics fields. Dr. Dave is a former vice president and director of Loctite Corp., and has spent many years troubleshooting adhesive and sealant problems. Questions for publication should be directed to him at 242 Trails End, Aurora OH 44202; (330) 562-2930; FAX (865) 251-9687; e-mail DrDave242@att.net ; or visit http://www.fldenterprises.com .

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40