In his February 2009 column, Dr. Dave discusses UV-cured coatings and water-based adhesives for laminating fine aluminum foil to paper.

Question: I am considering using a UV-cured coating for some irregularly shaped parts, however it is almost impossible to orient the parts so that the UV radiation cures all the coating; there will be areas that do not see the radiation. How can I cure these?

Answer: Talk to your suppliers about so-called “shadow curing” options. Most UV-cured coatings are based on acrylates and methacrylates, and they cure free-radically by the decomposition of a photoinitiator. However, it is possible to build in a secondary cure mechanism to cure the areas that do not get exposed to the UV radiation. Some allylic functional monomers will crosslink by exposure to atmospheric oxygen, and it is also possible to add isocyanate functionality to generate crosslinking by atmospheric moisture in much the same way one-component polyurethanes do.

Shadow curing systems can cure in times ranging from less than an hour to several days, depending on the system and your specific requirements. You will have to be careful about storage of these types of systems in order to minimize exposure to the atmosphere.



Question: I was wondering if you know where I can find a formula for a water-based adhesive for laminating fine aluminum foil to 23 lb paper. I am having a problem with the product wrinkling after it sets.

Answer: Water-based adhesives can be based on several polymers, including polyvinyl alcohol (PVOH), polyvinyl pyrrolidone (PVP), starches and cellulose derivatives. There are also emulsions such as those based on polyvinyl acetate (PVA) or ethylene vinyl acetate (EVA). Wrinkling is caused by the shrinkage of the adhesive due to evaporation of the water as it dries.

The real key to eliminating wrinkling is to use a very-high-solids system, or one with a minimum amount of water. Unfortunately, some manufacturers use a lot of water to increase the "open time,” or the period over which the adhesive is aggressively tacky and a successful bond can be made. However, this adversely increases paper wrinkling as the adhesive material dries and shrinks. Another method of decreasing wrinkling during drying is to replace water with less-volatile solvents such as glycols and other water-miscible solvents.

Links

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

Dunn

Q&A Exchange is written by Dave Dunn, Ph.D., of F.L.D.Enterprises, a technical consultancy and full-service industrial market-research firm specializing in the adhesives, sealants, specialty rubbers and plastics fields. Dave is a former vice president and director of Loctite Corp. and has spent many years in troubleshooting adhesive and sealant problems. Questions for publication should be directed to him at 242 Trails End, Aurora OH 44202; phone 330-562-2930; fax (330) 247-1690; or email DrDave242@windstream.net .

Recent Articles by Dave Dunn

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40