In his January 2009 column, Dr. Dave discusses epoxies and the differences between hardeners, primers, accelerators, and activators for adhesives and sealants.

Question: We want to use a flexible epoxy adhesive sealant for an application that will be exposed to daylight, but we are concerned about possible long-term discoloration of the product. Can you offer some advice?

Answer: Epoxies are rarely used in situations where constant light exposure is possible. For example, you may have noticed that epoxy coatings are normally used as primer coats and then top-coated with an acrylic or polyurethane. This is because epoxies tend to chalk and yellow when exposed to daylight. Use of proper pigmentation and UV absorbers can often help this situation, but the best solution is to get away from the traditional aromatic backbone of epoxy resins. The use of epoxies based on hydrogenated bisphenol A instead of straight bisphenol A will often solve this problem, albeit at a greater expense. Another alternative is to look at cycloaliphatic epoxy resins, though you may need to cure these with heat or UV radiation. Cycloaliphatic epoxies have been in short supply in recent years after a major manufacturer stopped production, but they are being offered again by a number of new suppliers.



Question: What is the difference between a hardener, a primer, an accelerator and an activator for adhesives and sealants?

Answer: This terminology can be confusing because the terms are often used interchangeably between technologies and differently by different manufacturers of the same technology. The term “hardener” is most often used in two-part epoxy adhesives where most manufacturers call the part that actually contains the epoxy molecule the “adhesive” and the part that contains the curing agent the “hardener.” Some of these epoxy systems also contain additives in the hardener component to speed up the cure; these are usually called “accelerators” or “catalysts.” Some one-component systems use so-called “primers” or “activators” that are applied to surfaces before applying the adhesive. Sometimes the primer will serve to condition the surface and ensure maximum adhesion - a good example is the use of organosilane primers for ensuring good adhesion and bond durability when RTV silicones are bonded to glass surfaces. In other cases, the primer or activator is actually used to speed up the curing of the adhesive. For example, special surface primers have been designed for surface-initiated adhesives (such as cyanoacrylates) to increase the speed of cure when atmospheric humidity is very low, or on so-called “inactive” surfaces.

I hope this helps, but unfortunately you will still find some confusion in the industry. When in doubt, ask your supplier specifically what a material actually does.

Links

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

Dunn

Q&A Exchange is written by Dave Dunn, Ph.D., of F.L.D.Enterprises, a technical consultancy and full-service industrial market-research firm specializing in the adhesives, sealants, specialty rubbers and plastics fields. Dave is a former vice president and director of Loctite Corp. and has spent many years in troubleshooting adhesive and sealant problems. Questions for publication should be directed to him at 242 Trails End, Aurora OH 44202; phone 330-562-2930; fax (330) 247-1690; or email DrDave242@windstream.net .

Recent Articles by Dave Dunn

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI June 2013 cover

2013 June

The 2013 June Adhesives and Sealants Industry Magazine includes articles about Nordson EFD and UV curing with lasers, as well as a case study on progressive cavity pumps. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40