In his July 2008 column, Dr. Dave discusses fire-retardant adhesives and the necessary approvals for sealants used on pipes carrying potable water.


Question: I typically deal with both epoxy and acrylic systems. Do you have any tips for making my adhesives fire retardant?

Answer: Fire retardants have historically been based on either inorganic materials or halogenated organic compounds. The entire subject of fire retardancy has been hotly debated in recent years because of the negative environmental aspects concerned with certain brominated materials. Phosphate and phosphonate compounds are typical alternative flame-retardants that do not make use of halogens. In adhesives, the choice of fire retardants is dependent on the type of system you are using. In a typical filled epoxy system, you can almost certainly use a combination of a solid inorganic fire retardant such as aluminum trihydate or magnesium hydroxide, perhaps supplemented by an organic one. However, if you have an unfilled acrylic system, particularly one with low viscosity, the choice of materials is much more limited. In this case, you might consider the handful of brominated or phosphorous-containing monomers that can be co-polymerized into the adhesive. There are several suppliers who specialize in fire retardants, and they can advise you on both product performance and safety aspects.



Question: What sort of approvals do I need for sealants used on pipes carrying potable water?

Answer: Sealants for contact with drinking water must be certified to a national standard called ANSI/NSF Standard 61. Several organizations are accredited by ANSI (American National Standards Institute) to test and certify this sort of product. The testing involves exposing the cured sealant to standardized test waters at specified temperatures and times and analyzing the extraction water for target contaminants. Results of this laboratory testing are then “normalized” to estimate their concentrations in specific pipe sizes or tanks, and a material will normally be certified for specific sizes and for specific water temperature use, defined as commercial hot water (180°F), “domestic” hot water (140°F), or cold water. The entire process of obtaining this certification can take many months, and I would advise reading the standard carefully before initiating testing so that you know the target contaminants and can determine whether or not your sealant has a good chance of passing the extraction testing.

Links

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

Dunn

Q&A Exchange is written by Dave Dunn, Ph.D., of F.L.D.Enterprises, a technical consultancy and full-service industrial market-research firm specializing in the adhesives, sealants, specialty rubbers and plastics fields. Dave is a former vice president and director of Loctite Corp. and has spent many years in troubleshooting adhesive and sealant problems. Questions for publication should be directed to him at 242 Trails End, Aurora OH 44202; phone 330-562-2930; fax (330) 247-1690; or email DrDave242@windstream.net .

Recent Articles by Dave Dunn

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40