AVERY DENNISON CORP.
This company has enhanced its Fasson Rapid-Roll product line with OPS (oriented polystyrene) shrink film. These transparent, oriented polystyrene films are reverse-printable and used for product decoration in medium-shrink applications. Narrow-web converters can now select from CD Shrink OPS 45 or CD Shrink OPS 55 products. These shrink film products offer excellent contoured package decoration with 360-degree printability.


More