Bostik HM7229 is a dimer polyamide-based hot melt adhesive. Offering immediate handling strength, this granular-form adhesive provides excellent adhesion to textiles, vinyl, wood and some plastics. Resistant to plasticizer migration and temperatures as high as 125ºC, HM7229 is recommended for many automotive-interior assembly tasks. Typical uses include wire-harness attachment in automotive headliners, interior trim attachment and wood bonding. It can also be applied robotically for headliner and carpet installation.