This company offers Michem(r) Prime EAA copolymer dispersions. The dispersions provide the functional advantages of solvent coating systems without the health, safety and environmental issues associated with solvent products. They are an excellent additive in binders for nonwovens, laminating adhesives, extrusion coatings and more. The dispersions exhibit excellent adhesion to metallic and cellulosic substrates. Circle No. 103