The plant produces Poly bd® hydroxyl terminated polybutadiene materials. Polybutadiene polyols typically react with isocyanates to produce high-performance urethanes that are used in adhesive and sealants, encapsulants, coatings, and other specialty applications. The polyols provide low-temperature flexibility, resistance to strong acids and bases, superior electrical properties, and a low moisture transmission rate.