ZEPHRYM PD 4974 is a low-VOC, high-performance polymeric dispersant designed for iron oxide pigments. The material reportedly offers excellent ability to provide formulation stability in systems containing iron oxide pigments. It shows improved dispersion stability compared to competitive materials.

In one laboratory test, the paint, comprised of 70% red iron oxide pigment by weight, an aqueous binder and 2% dispersant (Zephrym PD 4974 or competitive material), was compared for stability. The paint containing the competitive material separated after 120 hours (five days) at room temperature. The same paint formulated with Zephrym PD 4974 reportedly never separated, even after 60 days of testing, after which the test was concluded.

In addition to its ability to stabilize formulations, Zephrym PD 4974 can enhance color development and reduce or eliminate the level of thickeners in the formulation.

For more information, visit www.crodacoatingsandpolymers.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI August 2014 cover

2014 August

Our August issue includes what is traditionally our most popular article of the year: the ASI Top 25. You won't want to miss it!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px