CONAPOXY FR-1047/EA-87, FR-1047/DPEA-25652, and DPFR-29589/DPEA-25652 demonstrate excellent resistance to thermal shock, low exothermic temperatures, and outstanding arc resistance. In addition to having strong flame retardant characteristics, the systems are non-abrasive and provide low room temperature processing viscosity.
CONAPOXY FR-1047/EA-87 has a four-hour gel time and a mixed viscosity of 6,800 cps at 25ºC. CONAPOXY FR-1047/DPEA-25652 has a 90-minute gel time and a mixed viscosity of 4,000 cps at 25ºC, and FR-1047/DPFR-29589 has a 70-minute gel time and a mixed viscosity of 6,800 cps at 25ºC. All three products are filled with a non-abrasive filler to reduce wear on machine metering/dispensing.