The aluminum is coated on the other side with a pressure-sensitive silicone adhesive for a sure grip on metal, glass or ceramic surfaces.
The result, D/W 351, is a heat-resistant tape featuring PTFE’s chemical resistance, wide operating temperatures and a low coefficient of friction. The foil backing is comprised of a standard 3003 grade of aluminum. Properties are consistent because of the foil’s uniform thickness of 0.005” with a tolerance of +/- 5%.
DeWAL D/W 351 is used in applications like high volume heat-sealing equipment in food packaging and bagging, and as a limited-use wear strip. D/W 351 is available in widths from 0.5” to 12”. The roll length is 11 yards.