DEWAL INDUSTRIES INC.: HVOF Tape

This company has announced the availability of a one-step masking tape that masks products during extremely hot, highly abrasive high-velocity oxygen-fuel (HVOF) thermal spraying.

DeWAL D-Max is a pressure-sensitive tape tested to temperatures over 1000°F (538°C) and forces greater than Mach II. The backing and construction are proprietary. This product features a backing thickness of 0.028mils (0.635mm) and adhesion of 55 oz./inch.

DeWAL D-Max HVOF tape joins a large family of thermal spray tapes manufactured in DeWAL’s Saunderstown, RI, facility. Free of carbonizing materials, these tapes form protective masks against grit blast, ceramic spraying, plasma spraying and arc spraying.

DeWAL tapes are used by several prominent aircraft engine, automotive, medical and mission-critical manufacturers.  DeWAL thermal spray tapes come in many constructions (both single- and double-ply) and are sometimes die-cut.

D-Max is available in widths from 0.25 to 24.0 inches (6.35mm to 0.61m) in 18-yard (16.5m) lengths. The material is silver-grey in color.

All DeWAL tapes are tested according to ASTM standards and meet RoHS criteria. DeWAL is ISO 9001:2000 registered.

For more information, visit www.dewal.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI June 2013 cover

2013 June

The 2013 June Adhesives and Sealants Industry Magazine includes articles about Nordson EFD and UV curing with lasers, as well as a case study on progressive cavity pumps. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40