HM-2520 is a neutral-cure, low-VOC sealant that enables parts to be moved immediately upon application. It also offers higher tensile strength for applications that require more secure adhesion.
“HM-2520 Assembly Sealant helps maximize plant efficiency and production output by effectively removing cure time from the manufacturing process,” said Ross Noel, senior application engineer for Dow Corning.
HM-2520 has a high tensile strength of 700 psi and service temperatures ranging from –50o to 300oF. This product meets FDA Regulation CFR 177.2600 and is NSF 51 and NSF 61 listed.
For more information, visit www.dowcorning.com.