Easy-to-apply, the sealant provides unprimed adhesion on many substrates, making it an excellent solution for a number of industrial sealing and bonding applications.
Dow Corning 732 Multi-Purpose Sealant remains stable and flexible from -60° to 180°C (-76° to 356°F), with short peaks up to 205°C (401°F). This sealant complies with military specification MIL-A-46106 and meets FDA CFR 177.2600 standards.