DOW REICHHOLD: Tape Saturant Latex

This company has introduced DR1221 Tape Saturant, a specialty latex for use in high-performance masking tapes. The new latex delivers excellent tensile strength, water resistance and elongation properties for improved performance of tapes used in high-temperature applications.

According to test data that shows significant improvement in heat-aged properties compared to competitive saturants currently available, this new latex is an excellent choice for achieving a balanced set of performance properties in tapes used in demanding environments. These properties - including tensile strength and elongation performance - are especially important for applications such as automotive refinishing and electronic baking.

Dow Reichhold also markets DL219 latex and DL220 latex for a range of general-purpose tape and specialty paper applications.

For more information, visit www.dowreichhold.com/saturants.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40