DYMAX Cure-PointTM 9440-A/B cures to depth in seconds upon exposure to UV/visible light to provide protection to electronic components and circuitry. It is a UV/visible light-curable silicone potting and sealing material designed for applications where fast cure, enhanced thermal performance, and room-temperature shadowed-area cure are required. Cure-Point 9440-A/B has a >90 day room temperature mix life.

This product is designed to withstand long exposure to temperatures ranging from below -40°C to above 200°C while retaining fast-cure processing benefits associated with UV-curable materials. This makes it superior to RTV silicones and heat-cure silicones which require longer cure times or elevated temperatures to cure. Cure-Point 9440-A/B excels in applications where oil or chemical exposure are present. It also features a fast, tack-free cure with negligible shrinkage.

DYMAX UV/visible light-curable materials are solvent free and their ability to cure in seconds results in lower processing costs. When cured with DYMAX light-curing spot lamps, focused beam lamps or flood lamps, they deliver optimum speed and performance for maximum efficiency. This product is in full compliance with the RoHS Directives 2002/95/EC and 2003/11EC.

For more information, visit www.dymax.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40