Dynaloy, Inc., Indianapolis, has developed Dynasolve 2000, a solvent designed to remove cured polyurethane from micro-pore screens used in the polyurethane foam-blowing process. The product works at room temperature in a simple soaking tank. It is a safe solvent with a flash point greater than 200ºF. Even screens that are saturated with cured polyurethane are easily cleaned in less than one hour.