FRANKLIN ADHESIVES & POLYMERS: Contact Cement

Multibond® Contact Cement is a new adhesive that enables manufacturers of furniture and other laminated products to “go green” from beginning to end–with an adhesive that offers strong initial green grab while also helping keep the environment safe.

This company, a division of Franklin International, offers Multibond® Contact Cement, a new adhesive that enables manufacturers of furniture and other laminated products to “go green” from beginning to end–with an adhesive that offers strong initial green grab while also helping keep the environment safe.

Multibond contact cement is a solvent-free water-based neoprene formula that contains no VOCs. As such, it meets LEED requirements for indoor air quality (IAQ) and moves construction projects one step closer to coveted LEED certification. Although safe for the environment, the cement offers all the performance characteristics not always found in green adhesives: strong green grab; quick dry time; and high resistance to water, solvent and heat. Manufacturers can machine it almost immediately after application, speeding up production in their plants for increased efficiency. The ability to clean up this adhesive while it is still wet further reduces production time.

For more information, phone (800) 877-4583 or visit www.franklinadhesivesandpolymers.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI June 2013 cover

2013 June

The 2013 June Adhesives and Sealants Industry Magazine includes articles about Nordson EFD and UV curing with lasers, as well as a case study on progressive cavity pumps. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40