This company has introduced a polyether foam, cured-in-place gasketing material formulated for cost-effective automotive interior and exterior Buzz, Squeak & Rattle applications. The material adheres easily to a variety of substrates and cures at room temperature, with accelerated cure upon exposure to heat. A resilient, two-component black rubber foam, this gasketing material is very soft, offers excellent adhesion to hard-coated acrylic polycarbonate and is resistant to heat up to 120 deg C. Circle No. 107