HENKEL: Anaerobic Stick Product Line

Henkel Corp. has expanded its line of Loctite QuickStix semi-solid anaerobic threadlocking, thread-sealing and anti-seize products to include flange sealants, gasket dressings, and retaining compounds. Convenient and portable, all eight Loctite QuickStix products deliver the same proven performance characteristics of liquids, but will not leak or drip and can be easily transported, applied, and stored. The QuickStix line features three new products: Loctite QuickStix 534 Hi-Tack Gasket Dressing, which allows cut gaskets to be positioned and held in place while mating surfaces are aligned for assembly; Loctite QuickStix 548 Gasket Eliminator Flange Sealant, for the prevention of fluid or gas leaks on all types of rigid iron, steel and aluminum flanges; and Loctite QuickStix 668 Retaining Compound for the bonding of non-threaded cylindrical assemblies.

For more information, visit http://www.loctite.com or call (800) LOCTITE.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI June 2013 cover

2013 June

The 2013 June Adhesives and Sealants Industry Magazine includes articles about Nordson EFD and UV curing with lasers, as well as a case study on progressive cavity pumps. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40