Henkel Corp. has reformulated three Loctite® cyanoacrylates to offer improved performance and stability for bonding to a range of substrates. The reformulated versions of Loctite 4203TM, 4204TM and 4205TM Prism® Instant Adhesives withstand temperatures up to 250°F, fixture and cure more rapidly, and offer excellent impact and peel resistance.

Loctite 4203 Prism Instant Adhesive is a low-viscosity, clear cyanoacrylate formulation designed to bond close-fitting parts. Loctite 4204 Prism Instant Adhesive is a medium-viscosity, clear cyanoacrylate formulation for general-purpose bonding. Loctite 4205 Prism Instant Adhesives is a clear, sag-resistant gel cyanoacrylate formulation suitable for vertical or overhead applications and for use on porous surfaces.

These thermal-resistant, rubber-toughened, surface-insensitive cyanoacrylates cure rapidly on a range of substrates, including plastics, metals, rubber, fiberglass, neoprene, and more. They can be used in the assembly of electric motors, kitchenware, marine components, military devices, microelectronics and other industrial assembly applications.  They are also suitable for gasket bonding.

For more information, visit www.instant.loctite.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI August 2014 cover

2014 August

Our August issue includes what is traditionally our most popular article of the year: the ASI Top 25. You won't want to miss it!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px