Henkel’s aerospace group has announced the launch of Epsilon 99100, a benzoxazine RTM/VARTM resin system that has been optimized for aerospace applications. This innovative technology is described as an innovative and effective alternative to epoxy chemistry. Epsilon 99100 significantly enhances mechanical performance and durability while lowering the costs associated with composite structure during manufacture and service. This product represents the first of a family of aerospace composite resin systems that will be introduced in 2008.

The Epsilon 99100 resin system is stable at ambient temperatures for over a year as a one-part resin. This reduces the cost of processing, storage and shipment. Additional features include: a broad processing window; viscosity stability; low heat release during cure; improved UV resistance; and more.

For more information, visit www.henkelepsilonresin.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40